Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.76 - 23.62 kV/mm | 374.9 - 599.9 kV/in | |
Arlon Silicone Hose and Duct Material with Polyester Substrate (65390R042)
(discontinued **) Side one - uncured silicone, 0.005 in., -0.001(0.1 mm, -0.01); Substrate - 6500 Polyester Fabric, 0.038 in. (0.97 mm) nominal; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.042 in.. |