Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 22.6 - 59.0 kV/mm | 575 - 1500 kV/in | Average value: 36.2 kV/mm Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |