Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.9 kV/mm | 531 kV/in | ASTM D149 |
Covestro Petlon® 7530 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Under Hood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperat.. |
|||
Dielectric Strength | 20.9 kV/mm | 531 kV/in | ASTM D149 |
Ensinger ENSILON® 6/6 GF30 Extruded Nylon 6/6, 30% glass-fiber-reinforced (PA66)
(discontinued **) ENSILON 6/6 GF30 is a 30% glass-fiber-reinforced nylon 6/6 material whose important properties include high tensile and flexural strength, stiffness, excellent heat deflection, and superior abrasion.. |
|||
Dielectric Strength | 20.9 kV/mm | 531 kV/in | Short Time; ASTM D149 |
Plenco 6500 Phenolic, Briquette, Injection Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |