Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 19.2 kV/mm | 487 kV/in | |
ACC QGel 310 QSI Quantum Silicones High Strength Gel QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid.. |