Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 18.7 kV/mm | 476 kV/in | ASTM D149 |
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene |
|||
Dielectric Strength | 18.7 kV/mm | 476 kV/in | ASTM D149 |
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT.. |