Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 47.83 kV/mm | 1215 kV/in | |
Saint-Gobain CHR® SG03-10(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |