Polymer Property : Dielectric Strength = 47.5 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 47.5 kV/mm
1210 kV/in
ASTM D149
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..