Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.85 kV/mm | 47.0 kV/in | ASTM D149 |
Saint-Gobain Korel® K40-20 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Dielectric Strength | 1.85 kV/mm | 47.0 kV/in | ASTM D149 |
Saint-Gobain Korel® K40-30 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® mi.. |
|||
Dielectric Strength | 1.85 kV/mm | 47.0 kV/in | ASTM D149 |
Saint-Gobain Korel® K40-35 Medium Deflection Micro-cellular Polyurethane Foam Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc.. |