Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 47.0 kV/mm | 1190 kV/in | IEC 243 |
LG Chemical RS-650 ABS, Extrusion, General Purpose Information Provided by LG Chem |
|||
Dielectric Strength | 47.0 kV/mm | 1190 kV/in | |
Von Roll Isola IMI Varnish 271 Spirit Gum Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: |
|||
Dielectric Strength | 47.0 kV/mm | 1190 kV/in | Full-wave Impulse; ASTM D3426 |
DuPont™ Nomex® 414 Paper, 15 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Dielectric Strength | 47.0 kV/mm | 1190 kV/in | IEC 60243-1 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |