Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.7 - 18.1 kV/mm | 450 - 460 kV/in | Average value: 17.9 kV/mm Grade Count:5 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |