Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.72 - 20.67 kV/mm @Thickness 3.17 mm |
450.1 - 525.0 kV/in @Thickness 0.125 in |
Short time value |
Abatron AboCast/AboCure 8109-2 High melting point. Filled version.Processing: 100/10 pbw; 90 minute potlife; mix at 130-140°C (270 °F); cures in 16 h/120°C (250°F), 10 h/140°C (285°F), 8 h/160°C (320°F), 2 h/ 200°C (390°.. |