Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 175 kV/mm | 4450 kV/in | VDE 0303 |
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |