Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 6.20 - 17.4 kV/mm | 157 - 442 kV/in | Average value: 11.6 kV/mm Grade Count:21 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |