Dielectric Strength >= 44.2 kV/mm
>= 1120 kV/in
Caplinq LINQTAPE™ PIT1A
Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p..
Dielectric Strength >= 44.2 kV/mm
>= 1120 kV/in
Caplinq LINQTAPE™ PIT1S
Product Description: LINQTAPE™ PIT-Series is a high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. Additionally, it p..