Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.1 kV/mm | 434 kV/in | 60Hz, Short Time, dry; ASTM D149 |
Sumitomo Bakelite North America E 8353-706R-1 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Dielectric Strength | 17.1 kV/mm | 434 kV/in | Short Time; ASTM D149 |
Plenco 6500 Phenolic, Briquette, Transfer Molded PLENCO 06500 is a glass reinforced phenolic molding compound offering improved strength, dimensional stability, and excellent electrical properties. UL recognized under component file E40654. 06500 .. |
|||
Dielectric Strength | 17.1 kV/mm | 434 kV/in | |
Dow Corning 3110 SILICONE RUBBER ENCAPSULANT Two-part, white, condensation cure, moderate flow, general purpose encapsulant, cure speed varied by catalyst type and mix ratio.Information provided by Dow Corning |
|||
Dielectric Strength | 17.1 kV/mm | 434 kV/in | Wet, short term. ASTM D149 |
Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GI.. |