Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.2 kV/mm | 412 kV/in | S/T |
Abatron AboCast 8103-27 High-Performance Dielectric Epoxy AboCast 8103-27 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h.. |