Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 4.10 kV/mm | 104 kV/in | AC 60 Hz; 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 20GTR Thin-Film GTR Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of .. |