Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.7 - 155 kV/mm | 400 - 3940 kV/in | Average value: 50.2 kV/mm Grade Count:122 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |