Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.4 kV/mm | 392 kV/in | ASTM D149 |
DSM Biomedical Elasthane™ 75D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility
Elasthane™ TPU exhibits outstanding hydrolytic stabilit.. |