Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.4 - 14.2 kV/mm | 340 - 360 kV/in | Step by Step |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |