Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 36.7 kV/mm | 932 kV/in | IEC 60243-1 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |