Electrical Properties Metric English Comments
Dielectric Strength 80.0 - 140 kV/mm
2030 - 3560 kV/in
Average value: 116 kV/mm Grade Count:8
Overview of materials for Styrene-Butadiene Copolymer, SBC
This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values ..