Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 138 kV/mm | 3500 kV/in | ASTM D149 |
Rogers Corporation Ultralam® 3850 Liquid Crystalline Polymer Circuit Material ULTRALAM® 3850 laminate circuit materials utilize highly temperature resistant liquid crystalline polymer (LCP) as the dielectric film.Features & Benefits:Excellent high frequency propertiesStable .. |
|||
Dielectric Strength | 138 kV/mm | 3500 kV/in | ASTM D149 |
Cytec Conathane® CE-1164 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Dielectric Strength | 138 kV/mm @Frequency 60.0 Hz |
3500 kV/in @Frequency 60.0 Hz |
ASTM D150 |
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Dielectric Strength | 138 kV/mm | 3500 kV/in | 0.25 inch electrodes in dry air @25°C; ASTM D149-81 |
DuPont Teijin Films Melinex® S Polyester Film, 400 Gauge Melinex® S is a general purpose film which combines excellent handling characteristics with a slightly hazy appearance. It is available in specific thicknesses from 48 - 500 gauge, and is used for .. |
|||
Dielectric Strength | 138 kV/mm | 3500 kV/in | ASTM D149 |
3M Scotch-Weld™ DP807 Acrylic Adhesives 3M™ Scotch-Weld™ Acrylic Adhesive DP807 is a two-part, 1:1 mix ratio, toughened acrylic structural adhesives. They exhibit excellent shear and peel strengths along with good impact, durability and.. |
|||
Dielectric Strength | 137.8 kV/mm | 3500 kV/in | ASTM D149-95a |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Dielectric Strength | 138 kV/mm | 3500 kV/in | ASTM D149 |
Cytec Conathane® CE-1163 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |