Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.7 kV/mm @Thickness 0.965 mm |
347 kV/in @Thickness 0.0380 in |
|
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Sc.. |
|||
Dielectric Strength | 13.7 - 15.6 kV/mm | 347 - 397 kV/in | short time |
Bulk Molding Compounds BMC HT12-1026 Unsaturated Polyester Bulk Molding Compound BMC HT12-1026 is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid caps.. |
|||
Dielectric Strength | 13.7 - 15.6 kV/mm | 347 - 397 kV/in | short time |
Bulk Molding Compounds BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound BMC HT12-1023L is a highly engineered Unsaturated Polyester Bulk Molding Compound developed for automotive under-hood applications. This compound is specified by Ford motor company for solenoid cap.. |