Polymer Property : Dielectric Strength = 34.9 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 34.9 kV/mm
886 kV/in
ASTM D149
Arlon 44602W020W 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 1165 FiberglassProduct is designed to meet the FAR 25.853 App.F, P.1,.Aii flame resistance requirements b..