Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.4 kV/mm | 875 kV/in | |
Saint-Gobain CHR® SG03-14(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Dielectric Strength | 34.4 kV/mm | 875 kV/in | ASTM D1000 |
3M Scotch® 70 Self-Fusing Silicone Rubber Electrical Tape Scotch® 24 Brand 70 Silicone Rubber Electrical Tape is a high-temperature arc and track resistance tape composed of self-fusing, inorganic silicone rubber and easy-tear and easy-strip liner.Informa.. |
|||
Dielectric Strength | 34.4 kV/mm @Thickness 0.762 mm |
875 kV/in @Thickness 0.0300 in |
ASTM D149 |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |