Polymer Property : Dielectric Strength = 3333 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 131.2 kV/mm
3333 kV/in
Saint-Gobain CHR® M788 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Strength 131.2 kV/mm
3333 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Mylar® EC Polyester Film, 300 Gauge
Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta..
Dielectric Strength 131.2 kV/mm
3333 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Mylar® EL Polyester Film, 300 Gauge
Mylar® EL films, typically 48 through 500 gauge are strong, tough, general -purpose films for electrical/electronic uses. Heavier gauges of Mylar® EL films are similar to Mylar® MO films. Availab..
Dielectric Strength 131.2 kV/mm
3333 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Mylar® WC11/WC22 Polyester Film, 300 Gauge
Mylar® type WC11 films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectric and good handlin..
Dielectric Strength 131.2 kV/mm
3333 kV/in
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Mylar® WC Polyester Film, 300 Gauge
Mylar® WC films are general-purpose electrical grade films, similar to Mylar® EL. These clear to hazy films are tough and durable as a core wrap. They offer good dielectrics and good handling char..