Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 3.20 kV/mm | 81.3 kV/in | IEC 60243 |
Solvay TECHNYL® A 246M PA66, DRY Description: Unreinforced and modified polyamide 66, with very high impact resistance even at low temperature, for injection molding.Available in: Europe and North AmericaProduct Applications: TECHN.. |
|||
Dielectric Strength | 3.20 kV/mm | 81.3 kV/in | ASTM D149 |
Tipco Tipcolite® TMHS 291 Phenolic Compound, Khaki Cotton Fabric, in fluffy form, Soft Flow & High Impact Strength Soft Flow Phenolic Compound, Reinforced with Khakhi Cotton Fabric, in fluffy formApplications: Defence ApplicationsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Ind.. |