Electrical Properties Metric English Comments
Dielectric Strength 29.1 kV/mm
740 kV/in
ASTM D149
Polymer Resources NY6-GP1 General Purpose Nylon 6
General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry ..
Dielectric Strength 29.1 kV/mm
740 kV/in
ASTM D149
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized
General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
Dielectric Strength 29.1 kV/mm
740 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 201-55 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Dielectric Strength 29.1 kV/mm
740 kV/in
ASTM D149
Arlon 51106R015 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Dielectric Strength 29.1 kV/mm
740 kV/in
ASTM D149
Arlon 51146R015 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Dielectric Strength 29.1 kV/mm
740 kV/in
ASTM D149
Arlon 51276R015 Silicone Rubber/Fiberglass Laminate
Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Dielectric Strength 29.1 kV/mm
739 kV/in
ASTM D149
Arlon 51576R015D 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical v..