Electrical Properties Metric English Comments
Dielectric Strength 13.8 - 105 kV/mm
350 - 2670 kV/in
Average value: 28.7 kV/mm Grade Count:20
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
Dielectric Strength 90.0 - 105 kV/mm
2290 - 2670 kV/in
Air, 0.125mm Thk Tape; ASTM D149
Dalau Dalcon 086 100% Virgin PTFE modified polymer
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal ..
Dielectric Strength 90.0 - 105 kV/mm
2290 - 2670 kV/in
Air, 0.125mm Thk Tape; ASTM D149
Dalau Dalcon 086 100% Virgin PTFE modified polymer
Applications & Industries: General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs. Modified PTFE has an advantage over Homopolymer (Normal ..