Electrical Properties Metric English Comments
Dielectric Strength 1.06 kV/mm
26.9 kV/in
ICHS Fiberfax® Alumina-Silica Ceramic Fibers
Fiberfrax® ceramic fibers are made from high-purity alumina-silica materials. ICHS uses Fiberfrax® ceramic fiber to manufacture vacuum-formed products in:High-Temperature DuctworkCombustion C..