Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 10.1 kV/mm | 257 kV/in | Short Term per ASTM D149. |
Plenco Valite 1246-18X Novolac Phenolic, Granular, Injection Molded
(discontinued **) This Valite product has been replaced by Plenco 4246. Data provided by Plenco.VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, mol.. |
|||
Dielectric Strength | 10.1 kV/mm | 257 kV/in | Short Time; ASTM D149 |
Plenco 2408 Phenolic, Granular, Injection Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |