Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 25.9 kV/mm | >= 659 kV/in | ASTM D149 |
Arlon 56986XA028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Dielectric Strength | >= 25.9 kV/mm | >= 659 kV/in | ASTM D149 |
Arlon 56986R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |