Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 8.98 kV/mm | 228 kV/in | |
Aremco AREMCOLOX™ 502-1900-YTZP Dense Yttria Stabilized Zirconium Oxide This grade offers a high flexural strength for a zirconia. The fine grain size lends itself to be used in cutting tools where a very sharp edge can be achieved and maintained due to its high wear re.. |
|||
Dielectric Strength | 8.98 kV/mm | 228 kV/in | |
Aremco AREMCOLOX™ 502-1900-ZTA Dense Zirconia-Toughened Aluminum Oxide This grade is made up of > 80% alumina and the balance yttria stabilized zirconia (Y-TZP). Provides some of the advantages of pure Y-TZP at a reduced price. The addition of zirconia increases greatl.. |