Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 0.0984 kV/mm | 2.50 kV/in | ASTM D419 |
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |