Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 2.36 kV/mm | >= 60.0 kV/in | Compound; IEC 60243 |
Borealis Casico™ FR4805 Non Halogen Flame Retardant Compound for Sheathing Energy Cables Casico FR4805 is a thermoplastic, non-halogen containing natural jacketing compound. It combines high mechanical strength and toughness with flame retardancy. The composition of Casico FR4805 is b.. |
|||
Dielectric Strength | 2.36 kV/mm | 60.0 kV/in | ASTM D149 |
3M 4718 Single-Coated Foam Tape 3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast.. |