Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 185 kV/mm | 4700 kV/in | Value for a 1 mil sample.; ASTM D-149 |
Saint-Gobain Norton® PFA Fluoropolymer Film Features/Benefits:Outstanding flex life and stress crack resistancePerformance from -254°C (-425°F) to 260°C (500°F)Outstanding anti-stick release propertiesExcellent electrical properti.. |