Dielectric Strength 161 kV/mm
4090 kV/in
Von Roll Isola IMI Varnish 716 Solventless Polyester Varnish for Electrical Insulation
Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 56°C. Usag..