Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.9 - 15.5 kV/mm | 378 - 394 kV/in | ASTM D149-97a |
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer Somos® NeXT combines stiffness and impact resistance which brings it close the performance of injection molded thermoplastics. It produces finished parts with tight tolerances and detailed features.. |
|||
Dielectric Strength | 14.5 - 15.5 kV/mm | 368 - 394 kV/in | ASTM D149-97a |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |