Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.3 - 15.4 kV/mm | 363 - 392 kV/in | Average value: 15.0 kV/mm Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |