Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dielectric Strength = 1195 kV/in Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 47.05 kV/mm
1195 kV/in
ASTM D149
Arlon 99202R010 0.010" Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Cured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should no..