Electrical Properties Metric English Comments
Dielectric Strength 3.00 - 4.50 kV/mm

@Temperature 90.0 °C
76.2 - 114 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic ..