Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 111 kV/mm @Thickness 3.00 mm |
2820 kV/in @Thickness 0.118 in |
ASTM D149 |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |