Polymer Property : Dielectric Strength = 10.5 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 8.00 - 10.5 kV/mm

@Temperature 90.0 °C
203 - 267 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..
Dielectric Strength 8.00 - 10.5 kV/mm

@Temperature 90.0 °C
203 - 267 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..