Polymer Property : Dielectric Strength = 1.20 kV/mm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Strength 1.20 kV/mm

@Diameter >=3.00 mm
30.5 kV/in

@Diameter >=0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Parallel; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola G-Etronax M Melamine, Glass Fabric Reinforcement, White, Tubes
Description: Mechanical and electrical applications. Arc-resistant and tracking-resistant material. Good flame resistance. Self-extinguishing. Halogen-free. Lower high-voltage values and insulation ..