Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 5.2 arcs | 5.2 arcs | |
Struktol VP 3752 Flame retarded epoxy resin Applications: STRUKTOL VP 3752 is a difunctional epoxy resin, which contains a chemically bound organophosphorous substance. Thus the mechanical properties like tenacity and modulus are not influenc.. |