Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 4.0 arcs | 4.0 arcs | |
Struktol VP 3735 Flame retarded epoxy resin Applications: STRUKTOL VP 3735 is a multifunctional epoxy resin, which contains a chemically bound organophosphorous substance. Thus the mechanical properties like tenacity and modulus are not influ.. |
|||
High Amp Arc Ignition, HAI | 4.0 arcs | 4.0 arcs | |
Struktol VP 3742 S Flame retarded epoxy resin Applications: STRUKTOL VP 3742 is a polyfunctional epoxy resin which contains a chemically bound organo-phosphorous substance. Thus the mechanical properties like stability and modulus as well as ch.. |