Electrical Properties | Metric | English | Comments |
---|---|---|---|
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 920 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Lexan® PPC4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Ultem 1010FV PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contant compliant, NSF 51 listing.This data wa.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics ULTEM 1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics ULTEM 1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics ULTEM 1100F PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant. UL94 V0, V2 and 5VA listing. Effective June 2007, this grade will no longer be supported with biocompa.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Ultem 2212 PEI (Asia Pacific) 20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics ULTEM MD131A PEI Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) PBT + PC, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Valox® 508R PBT+PC 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-FR. Reduced warpage characteristics. Applications same as VALOX 420R. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Valox® 865 PBT+PET 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics NORYL PX1265 PPE+PS Automotive applications. Exterior mirror and cluster housings, speaker grilles, cowl tops, exterior trim. 270F (132C) DTUL. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | surface, PLC code 3; UL 746A |
SABIC Innovative Plastics Noryl BN30 PPE+PS Blowmoldable. DTUL 180F. UL rated.This data was supplied by SABIC-IP for the Americas region. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 3412ECR PC Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v.. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs | 15 - 30 arcs | UL 746A |
SABIC Innovative Plastics Lexan® 940 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. |
|||
High Amp Arc Ignition, HAI | 15 - 30 arcs @Thickness 3.00 mm |
15 - 30 arcs @Thickness 0.118 in |
ALL |
Hexion Bakelite™ PF 2855 Phenolic Formaldehyde Resin, High Surface Quality, Low Shrinkage, For Electrostatic Coating, Dishwasher Proof, UL Listed Phenolic molding compound, inorganically/organically filled, heat resistant up to 250°C, hot steam and hot water resistant, high surface quality, for electrostatic coating, UL listed molding compou.. |