Polymer Property : High Amp Arc Ignition, HAI = 14.0 arcs Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Amp Arc Ignition, HAI 14.0 - 120 arcs
14.0 - 120 arcs
Average value: 44.5 arcs Grade Count:4
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..