Electrical Properties | Metric | English | Comments |
---|---|---|---|
Hot Wire Ignition, HWI | 0.00 - 7.0 sec @Thickness 1.50 mm |
0.00 - 7.0 sec @Thickness 0.0591 in |
UL 746A |
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications. |
|||
Hot Wire Ignition, HWI | 0.00 - 7.0 sec | 0.00 - 7.0 sec | UL 746A |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |